Dalam tempoh 2 bulan, defect ini muncul lg. Thin spot bg product ini blaku kerana bberapa sbb:
1. Viscosity dope rendah - tmbh thickener
2. Wetting pada former kurang baik-leh tmbh wetting agent
3. CN yg rendah
4. Froth level yg kurang - kurang lancar coating